اکسید روی 800 اکسید روی کد 800 (Data Sheet) جهت چاپ برگ آنالیز اینجا کلیک نمایید Description Reference shokuhieh method Specification Unit Properties No ………………… SQ-201 Min 99.8 % Purity of zinc oxide 1 ASTM D 4315 --- Max 0.003 % Sieve Residue on 325 Mesh 2 ASTM C25 --- Max 0.4 % Loss on Heating 3 ISO 7888 --- Max 90 µs/cm Electric Conductivity 4 ISIRI 8524 --- Max 230 ppm Lead Content 5 ISIRI 8524 --- Max 20 ppm Cadmium Content 6 ISIRI 8524 --- Max 5 ppm Manganese Content 7 ISIRI 8524 --- Max 10 ppm Copper Content 8 ISIRI 8524 --- Max 10 ppm Iron Content 9 ISIRI 8524 --- Max 5 ppm Cobalt content 10 ISIRI 8524 --- Max 5 ppm Nickel Content 11 ISIRI 8524 --- Max 15 ppm Aluminium Contant 12 ………………… SQ-209 …………………. m 2/g Nitrogen Surface Area/BET 13 ………………… SQ-204 Nodular Crystal Structure 1300X 14 ………………… SQ-203 ok Whiteness 15 ………………… SQ-205 ………………… % Total Sulfur Content 16 ………………… SQ-206 Max 90 Par/10gr Metalic Zinc Test 17 ………………… SQ-208 m2/gr Specific Surface Area 18 ………………… SQ-207 Min1250 mesh Mesh Particle size 19 ASTM D 1817 ---- Min 0.56 gr/cm3 Bulk density 20